1 to 10 of 227 Results
Jun 4, 2024
Wagner, Jonas; Hagenlocher, Christian; Weber, Rudolf; Hummel, Marc; Beckmann, Felix; Moosmann, Julian; Graf, Thomas, 2024, "Synchrotron X-ray video of full-penetration laser welding of aluminum AA1050A", https://doi.org/10.18419/darus-3860, DaRUS, V1
The video shows a synchrotron x-ray video of full-penetration laser welding of the aluminum alloy AA1050A (Al99.5). At the beginning of the video the transition from partial penetration welding with a keyhole which is closed at its bottom to full-penetration welding with a keyhol... |
AVI Video - 102.5 MB -
MD5: e21773391657105dd416987e3988df1f
|
Jun 4, 2024
Hinterkopf, Christoph, 2024, "Data for: "Influence of beam parameters on the capillary formation in partial and full penetration in high speed laser beam welding of metals"", https://doi.org/10.18419/darus-2111, DaRUS, V1
In this experiment copper and aluminum were partially and fully penetrated at high speed with a laser beam. The structure as well as the depth of the capillary were filmed with an X-Ray machine. The video footage were used to reconstruct and later ray traced to analyse the therma... |
PNG Image - 264.5 KB -
MD5: 510d82b2b9b43d4a7c308b6401a07fae
capillary formation of a laser welding process in aluminium AlMg3, spot diameter 100 µm |
PNG Image - 340.0 KB -
MD5: 58eebd9e7d6abc504444435a8185092a
capillary formation of a laser welding process in a 1 mm thick sheet of copper Cu K75, spot diameter 100 µm |
Adobe PDF - 2.3 MB -
MD5: 3295137fe671a07a0acc7b727cdf5e55
PDF version of Laborbuch_IFSW-21-12.xslx |
MS Excel Spreadsheet - 9.9 MB -
MD5: 42dc822b0ca19b79f2bceeb4618bec9f
experimental/evaluation table |
MS Excel Spreadsheet - 15.4 KB -
MD5: 8b68ec3b1258a005bb333cddfe7d7836
scale table X-Ray images |
Adobe PDF - 577.9 KB -
MD5: 1bb44deea1a5fdb205b71e96bbb773fb
PDF version of Maßstab Röntgenaufnahmen IFSW-2112.xslx |
PNG Image - 1.1 MB -
MD5: 8e2b5f23f8662b1c047f113cc5b815af
Experimental setup |