1 to 10 of 184 Results
PNG Image - 264.5 KB -
MD5: 510d82b2b9b43d4a7c308b6401a07fae
capillary formation of a laser welding process in aluminium AlMg3, spot diameter 100 µm |
PNG Image - 340.0 KB -
MD5: 58eebd9e7d6abc504444435a8185092a
capillary formation of a laser welding process in a 1 mm thick sheet of copper Cu K75, spot diameter 100 µm |
PNG Image - 1.1 MB -
MD5: 8e2b5f23f8662b1c047f113cc5b815af
Experimental setup |
JPEG Image - 10.5 MB -
MD5: 094934ec1733f34bc842e202751bce3f
|
JPEG Image - 155.8 KB -
MD5: 43a7b582a61f94c26821cafa8cae60a2
|
JPEG Image - 9.3 MB -
MD5: 0e555e5510a33872d988421a4bd1fd49
|
JPEG Image - 11.0 MB -
MD5: 2b3dc1436e757892a9c739e55b477f4f
|
JPEG Image - 3.3 MB -
MD5: e72192bdaa67497feb746778aaf3771f
|
JPEG Image - 10.1 MB -
MD5: 774d70df599e43234f5d6ee847b1436e
|
JPEG Image - 3.0 MB -
MD5: 9ce5df4aef40a688b3479795b140ed3d
|